Referensi teknis

Padanan material fitting pipa

Tim pengadaan luar negeri umumnya menetapkan grade ASTM/ASME; proyek Eropa memakai EN/DIN; proyek Jepang/Korea memakai JIS; proyek Tiongkok memakai GB. Halaman ini merangkum padanan paling sering ditanyakan untuk fitting, flange, dan pipa.

36 hasil

Carbon-steel butt-welding fittings

Elbows, tees, reducers, caps for moderate-to-high-temperature service.

  • ASTM/ASME: A234 / SA234
  • EN: EN 10253-2 (P235GH/P265GH)
  • JIS: JIS B2311 / B2312
  • GB: GB/T 12459 (材质 GB/T 700)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
WPBP235GH (1.0345)STPG37020≤ 425°C, general carbon steelTawar
WPCP265GH (1.0425)STPG410Q345Higher tensile, ≤ 425°CTawar

Alloy-steel butt-welding fittings (high temperature)

Cr-Mo creep-resistant alloys for high-temperature steam, refinery, power plant.

  • ASTM/ASME: A234 / SA234
  • EN: EN 10253-2 / 10216-2
  • JIS: JIS G3203 / G3458
  • GB: GB/T 12459 (材质 GB/T 5310)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
WP116Mo3 (1.5415)STPA1215Mo3≤ 530°CTawar
WP1113CrMo4-5 (1.7335)STPA2212CrMo / 15CrMo≤ 580°CTawar
WP1211CrMo9-10 (1.7383)STPA2312Cr2Mo≤ 580°CTawar
WP2210CrMo9-10 (1.7380)STPA2412Cr2Mo / 12Cr2Mo1≤ 600°CTawar
WP5X11CrMo5 (1.7362)STPA251Cr5Mo≤ 650°C, sulfideTawar
WP9X11CrMo9-1 (1.7386)STPA261Cr9Mo≤ 650°CTawar
WP91X10CrMoVNb9-1 (1.4903)STPA28 / SUS410J310Cr9Mo1VNbN≤ 625°C, supercriticalTawar

Stainless-steel butt-welding fittings

Austenitic 304/316/321/347 corrosion-resistant fittings.

  • ASTM/ASME: A403 / SA403
  • EN: EN 10253-4
  • JIS: JIS B2311 (材质 JIS G3459)
  • GB: GB/T 12459 (材质 GB/T 14976)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
WP304 / 304LX5CrNi18-10 (1.4301) / X2CrNi19-11 (1.4306)SUS304 / SUS304L0Cr18Ni9 / 022Cr19Ni10General corrosionTawar
WP316 / 316LX5CrNiMo17-12-2 (1.4401) / X2CrNiMo17-12-2 (1.4404)SUS316 / SUS316L0Cr17Ni12Mo2 / 022Cr17Ni12Mo2Chloride / acid serviceTawar
WP321X6CrNiTi18-10 (1.4541)SUS3210Cr18Ni10Ti≤ 800°C, Ti-stabilizedTawar
WP347X6CrNiNb18-10 (1.4550)SUS3470Cr18Ni11Nb≤ 850°C, Nb-stabilizedTawar
WP310X8CrNi25-21 (1.4845)SUS310S0Cr25Ni20High-temp, scaling resistanceTawar
WP-DS (Duplex 2205)X2CrNiMoN22-5-3 (1.4462)SUS329J3L022Cr22Ni5Mo3NPitting / chlorideTawar

Low-temperature carbon / alloy fittings

LNG, cryogenic and arctic pipelines.

  • ASTM/ASME: A420 / SA420
  • EN: EN 10253-2 (P275NL2 / P355NL1)
  • JIS: JIS G3204 (SLA-series)
  • GB: GB/T 12459 (材质 GB 6479 16MnDR)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
WPL6P275NL2 (1.1104)SLA235A16MnDR≥ –50°CTawar
WPL3P355NL2 (1.1106)SLA325B09MnNiDR≥ –100°CTawar
WPL911MnNi5-3 (1.6212)SLA46006MnNiMoDR≥ –196°C, LNGTawar

Carbon-steel forged flanges

Forged carbon flanges per ASME B16.5 / B16.47.

  • ASTM/ASME: A105 / SA105 / A350
  • EN: EN 10222-2 (P250GH/P280GH)
  • JIS: JIS G3202 (SF440A/SFVC1)
  • GB: GB/T 9112 (材质 NB/T 47008 20)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
A105 / SA105P250GH (1.0460)SF440A / SFVC120 / 25General forged carbonTawar
A350 LF2P280GH / 11MnNi5-3 (1.6210/1.6212)SFL216MnDRLow-temp ≥ –46°CTawar
A350 LF311MnNi5-3 (1.6212)SFL309MnNiDRLow-temp ≥ –100°CTawar

Alloy-steel forged flanges

Cr-Mo forged flanges for high-temperature/high-pressure piping.

  • ASTM/ASME: A182 / SA182
  • EN: EN 10222-2
  • JIS: JIS G3203 (SFVA)
  • GB: GB/T 9112 (材质 NB/T 47008)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
F11 / F11 Cl.213CrMo4-5 (1.7335)SFVA F11A1.25Cr-0.5Mo≤ 593°CTawar
F2210CrMo9-10 (1.7380)SFVA F22A2.25Cr-1Mo≤ 600°CTawar
F5X11CrMo5 (1.7362)SFVA F5A5Cr-0.5MoSulfide serviceTawar
F91X10CrMoVNb9-1 (1.4903)SFVA F9110Cr9Mo1VNbN≤ 625°C, ultra-supercriticalTawar

Stainless-steel forged flanges

Austenitic forged flanges per ASME B16.5.

  • ASTM/ASME: A182 / SA182
  • EN: EN 1092-1 (材质 EN 10222-5)
  • JIS: JIS G3214 (SUSF)
  • GB: GB/T 9112 (材质 GB/T 1220)
ASTM / ASMEEN / DINJISGBKondisi pemakaian
F304 / F304L1.4301 / 1.4306SUSF304 / SUSF304L0Cr18Ni9General corrosionTawar
F316 / F316L1.4401 / 1.4404SUSF316 / SUSF316L0Cr17Ni12Mo2Chloride serviceTawar
F3211.4541SUSF3210Cr18Ni10Ti≤ 800°CTawar
F51 (Duplex 2205)1.4462SUSF329J3L022Cr22Ni5Mo3NPitting / chlorideTawar

Seamless carbon-steel pipes

Seamless steel pipes for pressure and structural service.

  • ASTM/ASME: A106 / A53 / API 5L
  • EN: EN 10216-2
  • JIS: JIS G3454 / G3456
  • GB: GB/T 8163 / GB 5310
ASTM / ASMEEN / DINJISGBKondisi pemakaian
A106 Gr.BP235GH / P265GHSTPG370 / STPG41020Pressure pipingTawar
A53 Gr.BS195T / S235JRHSTPG370Q235BStructural / utilityTawar
API 5L X42-X70L290-L485L290-L485Oil & gas linepipeTawar

Stainless-steel pipes

Seamless / welded austenitic stainless pipes.

  • ASTM/ASME: A312 / SA312
  • EN: EN 10216-5
  • JIS: JIS G3459
  • GB: GB/T 14976
ASTM / ASMEEN / DINJISGBKondisi pemakaian
TP304 / TP304L1.4301 / 1.4306SUS304TP / SUS304LTP0Cr18Ni9 / 022Cr19Ni10General corrosionTawar
TP316 / TP316L1.4401 / 1.4404SUS316TP / SUS316LTP0Cr17Ni12Mo2 / 022Cr17Ni12Mo2Chloride serviceTawar
TP3211.4541SUS321TP0Cr18Ni10TiStabilized, ≤ 800°CTawar
TP347H1.4912SUS347HTP0Cr19Ni10NbN≤ 850°C, creepTawar

Search-ready answers

Common standards, material and inspection questions

These short answers help engineers confirm whether a fitting, flange or certificate requirement belongs in the RFQ before sending drawings.

What is MSS SP-25 used for?

MSS SP-25 is the marking standard for valves, fittings, flanges and unions. For pipe fittings and flanges it is normally checked together with the product standard, material grade, heat number, manufacturer mark and MTC traceability.

MSS SP-25markingheat number
View related products

What does JIS B2220 cover?

JIS B2220 covers steel pipe flanges used in Japanese projects. When replacing or quoting JIS flanges, confirm pressure rating, facing, bolt pattern, material grade and whether the project needs EN 10204-style material certification.

JIS B2220flangespressure rating
View related products

When should ASME B31.1 or ASME B31.3 be applied?

ASME B31.1 is commonly used for power piping such as boiler external piping and power-plant systems. ASME B31.3 is commonly used for process piping in refinery, chemical and industrial plants. Final selection follows the project design code.

ASME B31.1ASME B31.3design code
View related products

What material is ASTM A234 WPB?

ASTM A234 WPB is a wrought carbon-steel fitting grade for moderate and high-temperature pressure piping. It is commonly used for elbows, tees, reducers and caps matched with A106 Gr.B pipe and A105 forged flanges.

A234 WPBcarbon steelB16.9
View related products

What is the difference between EN 10204 3.1 and 3.2 MTC?

EN 10204 3.1 MTC is issued by the manufacturer with test results traceable to the batch. EN 10204 3.2 adds independent buyer or third-party inspection witness, which is often required for critical EPC, pressure-equipment and offshore projects.

EN 10204MTC 3.1MTC 3.2
View related products

What do RT, UT, MT and PT mean in piping inspection?

RT is radiographic testing, UT is ultrasonic testing, MT is magnetic particle testing and PT is liquid penetrant testing. The exact percentage and acceptance criteria must follow the drawing, ITP and applicable code.

RTUTMTPT
View related products

Rentang Manufaktur

Yang sebenarnya kami produksi sendiri

Standar di atas adalah kode yang kami patuhi. Di bawah adalah rentang dimensi dan kapasitas yang dapat kami kirim dari pabrik kami.

Rentang DN fitting buttweld

DN 15 — DN 1500

ASME B16.9 / EN 10253 / MSS SP-75

OD flensa maks

5 m

Tempaan + dimesin; ASME B16.47 Series A/B + EN 1092-1

Tonase tempaan maks

50 t

Tempaan khusus, blok, blank OD besar

Cakupan kelas tekanan

PN 6 — PN 400 / Class 150 — 2500

Class 150 / 300 / 600 / 900 / 1500 / 2500 (ASME B16.5 / B16.47); PN 6 - PN 400 (EN 1092-1)

Penafian

Tabel padanan ini disusun dari standar publik dan hanya untuk referensi teknis. Spesifikasi material akhir harus mengikuti jadwal teknis kontrak, standar wajib yang berlaku (PED, ASME, CE, dll.), dan tinjauan oleh insinyur material yang berkualifikasi.